The improvement of lifespan relies on process combination: steel upgrading, heat treatment standardization, cooling optimization, and maintenance ledger in four steps.

1、 Marginal benefits of steel upgrading

By increasing the chromium content from 3% to over 5%, the thermal fatigue life can be extended by about 25%.

Upgrading steel has increased the cost of molds by about 10% to 15%, but the cost of molds has decreased significantly.

After exceeding 6% chromium content, the revenue slows down and the marginal return on investment decreases.

2、 Standardization of heat treatment

By tempering twice and controlling the hardness between 48 and 52HRC, the early cracking rate can be reduced by about 35%.

Excessive quenching and cooling speed can easily generate internal stress, and the crack initiation time is advanced by about 20%.

The heat treatment curve and hardness record should be retained as delivery documents.

3、 Cooling and stress

The temperature difference on the mold surface decreased from 15 degrees Celsius to 5 degrees Celsius, and the crack initiation time was delayed by about 20%.

Adding a cooling point to the hot section causes a local temperature drop of about 25 degrees Celsius, and the peak thermal stress decreases synchronously.

When the cooling water flow is insufficient, the mold life may be shortened by more than 30%.

4、 Maintenance and ledger

Performing polishing and crack inspection every 5000 molds can extend the lifespan by approximately 10%.

If the carbon accumulation in the cavity exceeds 0.1 millimeters, it will increase the heat load and needs to be cleaned in a timely manner.

Xinfeng provides a template for the module ledger, which records temperature, pressure, and maintenance items on a weekly basis.

5、 Failure and mold replacement

Three consecutive cracks with a depth exceeding 1.5 millimeters enter the mold replacement window.

When the size drift exceeds 0.3 millimeters, it is mostly due to cavity creep, and the yield rate will drop below 90%.

Industry practice shows that when four actions are combined, the actual lifespan can be increased by about 40%.

Conclusion and Outlook

Life expectancy is not bought, it is managed.

Steel and heat treatment have upper limits, and cooling and maintenance determine whether it can approach the upper limit.

Extension: Calculation of Return on Investment for Life Extension

The upgrade of steel has increased the cost of a single set by about 12%, increased its lifespan by 25%, and reduced the cost of a single module by about 9%.

The investment in point cooling renovation is about 6% of the mold cost, with a 12% reduction in cycle time, and usually recoups the cost within six months.

The manual cost of the ledger system is about half an hour per hour, resulting in a 30% reduction in downtime.

The comprehensive return of three overlapping factors is usually visible within a product lifecycle.

When only making a single investment, the return is often lower than expected.

Recording inputs and outputs on a monthly basis makes it clear whether the life extension plan is worth continuing.

Addendum: Four specific actions for extending lifespan maintenance

Polishing the cavity to remove microcracks can extend its usage by approximately 2000 cycles per use.

When the hardness of the cooling water is high, scaling occurs faster, and installing a softening device can extend the maintenance cycle.

Insufficient lubrication of the ejector pin can increase local stress and make the edges of the mold cavity more prone to breakage.

Evaluating lifespan by module segmentation is closer to the true state than making a one-time judgment.

Addendum 2: Three Priority Orders for Life Extension Measures

Prioritize optimizing cooling, achieve quick results with minimal investment, and significantly increase lifespan after improving temperature difference.

Secondly, standardizing heat treatment with moderate investment can solve most early cracking problems.

Finally, considering the replacement of steel, the investment is relatively high and the marginal revenue is relatively low.

FAQ

How much longer can replacing steel extend its lifespan? If the chromium content is increased to over 5%, it will be extended by about 25%.

What is the hardness range? 48 to 52HRC is relatively stable.

Should heat treatment records be retained? Suggest delivering with the mold.

How much longer can a decrease in temperature difference extend lifespan? The delay from 15 degrees to 5 degrees is about 20%.

How often is the cavity checked? Suggest every 5000 cycles.

How thick is the carbon deposit that needs to be cleaned? If it exceeds 0.1 millimeters, it needs to be dealt with.

When should we change the mold? The crack depth exceeds 1.5 millimeters and the size drift exceeds 0.3 millimeters.

The Influence of Aluminum Liquid Temperature on Aluminum Alloy Casting Molds: How to Control Around 700 Degrees

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1502.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.