Perguntas frequentes

The core of thermal balance is the identification of heat nodes, zone temperature control, and beat stability.

  • Vistas: ...
  • Tempo de liberação: 2026-11-16

The core of thermal balance is the identification of heat nodes, zone temperature control, and beat stability.

1、 Identify hot spots first

The hot zone is a concentrated area of wall thickness, with solidification hysteresis, and the mold temperature is often more than 30 degrees Celsius higher than that of the thin-walled zone.

Using solidification simulation to locate hot spots is more accurate than relying on experience.

Without heat treatment, shrinkage and mold sticking will occur simultaneously.

2、 Partition temperature control

The mold temperature for thin-walled areas is set at 280 to 320 degrees Celsius, while for thick walled areas it is set at 340 to 380 degrees Celsius.

Partition independent temperature control can reduce the temperature difference of the mold surface from 15 degrees Celsius to within 5 degrees Celsius.

Xinfeng's molds are arranged with independent water circuits and thermocouples according to the hot section, supporting zone adjustment.

3、 Stable rhythm

A beat fluctuation exceeding 15% will disrupt the thermal balance and cause the mold temperature to drift accordingly.

Record the mold temperature every 30 minutes during continuous production, and adjust if the deviation exceeds 8 degrees Celsius.

Control the temperature rise of the cooling water within 5 degrees Celsius to avoid overcooling at the end.

4、 Structure and insulation

Adding insulation board around the mold can reduce the temperature drop at the edge of the mold surface by about 10 degrees Celsius.

Add insulation pads between the mold cavity and the press to reduce heat loss.

Spray release agent evenly, excessive spraying in certain areas can cause an increase in temperature difference.

5、 Verification method

Measure the temperature field using infrared thermography or embedded thermocouples, with a grid spacing of 50 millimeters.

When the measured temperature difference deviates from the design by more than 30%, the waterway and insulation should be rechecked.

Industry data shows that after optimizing the heat balance, the scrap rate can be reduced by about 20%.

Conclusion and Outlook

The temperature difference is not solved by increasing the water volume, but by zoning and insulation.

First locate the hot spot, then divide the temperature control into zones, and finally stabilize the rhythm. Three steps can achieve a stable temperature of plus or minus 5 degrees.

Extension: Three Sequence of Thermal Balance Adjustment

Adjusting the water temperature first and then the flow rate, reversing the order will mask the real problem.

The flow adjustment range increases by 10% each time to avoid overshoot.

Finally, adjust the spraying amount, and the change of spraying will immediately change the mold surface temperature.

Adjusting in this order usually takes 2 to 3 shifts to achieve the target temperature difference.

When there is no thermal imager, contact thermocouples can be used to measure point by point, with a grid of 50 millimeters.

After adjustment, record the parameter combination, which can be directly reused when changing models.

Addendum: Four parameters for temperature difference control

If the temperature difference is too large, the hardness difference of the same batch of parts will exceed 15HB, and the machining will increase the number of knives accordingly.

Adding insulation board to the hot zone can reduce heat dissipation by about 10%, which is more balanced with point cooling.

Cooling water is calculated at 8 liters per minute per branch, and insufficient total volume will lower overall efficiency.

The temperature records are saved by shift, making it easy to trace and adjust in case of abnormalities.

Addendum 2: Three records of thermal balance debugging

Record the flow rate of each branch and the temperature difference between the inlet and outlet. If the flow rate of a single branch is less than 8 liters per minute, it needs to be checked.

The mold surface temperature is measured according to the grid, and if the deviation exceeds 10 degrees Celsius, the spraying or water volume should be adjusted.

The rhythm and mold temperature are recorded synchronously, and the rhythm fluctuation often appears before the temperature anomaly.

Addendum 3: Two arrangements of temperature control components

The thermocouple should be buried at a distance of 5 to 10 millimeters from the surface of the cavity, with a reading delay of about 3 seconds if it is too deep.

At least one temperature measurement point should be set up in each area, and a single point layout cannot reflect the temperature difference.

FAQ

How much higher is the thermal section compared to the thin-walled area? Often above 30 degrees Celsius.

How much temperature difference can be controlled on the mold surface? Partition temperature control can reach plus or minus 5 degrees Celsius.

What is the mold temperature for thin-walled areas? 280 to 320 degrees Celsius.

How much rhythm fluctuation needs to be adjusted? Exceeding 15% disrupts thermal equilibrium.

How often is the mold temperature recorded? Continuous production is recommended every 30 minutes.

How much temperature drop can insulation board reduce? The edge is reduced by about 10 degrees Celsius.

How to verify temperature difference? Infrared thermography or embedded thermocouple measurement.

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1501.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.