Perguntas frequentes

The core parameters of mold steel and heat treatment are chromium content, hardness range, and tempering times.

  • Vistas: ...
  • Tempo de liberação: 2026-11-16

The core parameters of mold steel and heat treatment are chromium content, hardness range, and tempering times.

1、 Steel selection based on working conditions

When the chromium content of hot work die steel is higher than 5%, its thermal fatigue resistance is about 40% higher than that of ordinary steel.

It is recommended to choose steel grades with better thermal stability for large-scale continuous production, with a unit price about 15% higher.

Small batch and multi variety projects can use universal hot work steel, which can reduce costs by about 20%.

2、 Hardness range

The hardness of the cavity is usually controlled at 48 to 52HRC, balancing wear resistance and crack resistance.

When the hardness exceeds 55HRC, the risk of edge breakage increases and the crack propagation speed accelerates by about 1.4 times.

When the hardness is below 45HRC, the cavity is prone to collapse and the lifespan may be shortened by 30%.

3、 Heat treatment process

After quenching, perform two tempering processes, with each holding time calculated as 1 hour for every 25 millimeters of cross-sectional thickness.

Insufficient tempering will result in residual internal stress, and the probability of early cracking will increase by about 35%.

Xinfeng requires the supplier to provide heat treatment curves and hardness testing records, which will be delivered with the mold.

4、 Surface treatment and coating

The cavity can be treated with nitriding, with a layer depth of 0.02 to 0.05 millimeters, and the wear resistance is significantly improved.

Coating thickness exceeding 0.05 millimeters is prone to peeling, which can actually cause mold sticking.

The surface roughness is Ra1.6, and when combined with coating, it can reduce demolding resistance by about 15%.

5、 Failure judgment

If there are network cracks in the cavity with a depth exceeding 1 millimeter, it is usually judged as thermal fatigue failure.

If the measured hardness is lower than the design value by more than 3HRC, the heat treatment batch should be traced.

Industry data shows that molds with complete heat treatment records have an early failure rate that is about 30% lower.

Conclusion and Outlook

Steel determines the upper limit, and heat treatment determines whether the upper limit can be reached.

Requesting material certification and heat treatment curves during procurement is more meaningful than just looking at the brand.

Extension: Four verifications in steel procurement

Verify the steel grade and composition report, and ensure that the measured chromium content is consistent with the nominal value.

Verify the number of hardness measurement points, and it is recommended to have no less than 3 points for the same block.

Verify the number of tempering cycles and insulation time. If the curve is missing, it is considered that the process is unclear.

Verify the streamline direction of steel forgings. Misalignment in direction will reduce the crack resistance of the mold cavity.

If two or more of the four items are missing, the lifespan commitment is usually difficult to fulfill.

Writing the verification requirements into the procurement contract will make the supplier's quotation closer to the actual cost.

Addendum: Three Process Preparations for Steel Selection

Different steel grades can be used for different inserts of the same mold, and materials with better heat resistance should be selected in the hot spot area.

Steel forgings require ultrasonic testing, as internal inclusions can cause early cracking of the mold cavity during the batch stage.

Performing stress relief annealing before cavity processing can reduce subsequent deformation by approximately 0.1 millimeters.

Addendum 2: Two Requirements for Hardness Testing

It is recommended to measure at least 3 points on the same block and record their positions. Single point data cannot represent the overall hardness.

Hardness testing should be conducted 24 hours after tempering, as premature measurements may result in higher readings.

FAQ

What is the chromium content that is good for heat fatigue resistance? More than 5% is more appropriate.

What is the hardness of the cavity? Usually take 48 to 52 HRC.

What are the risks of high hardness? Exceeding 55HRC is prone to edge breakage.

How many times has it been tempered? Suggest twice, calculate the insulation time according to the thickness.

How deep is the nitride layer? 0.02 to 0.05 millimeters.

What happens if the coating is too thick? More than 0.05 millimeters are prone to peeling and sticking to the mold.

How to determine thermal fatigue failure? The depth of the network crack exceeds 1 millimeter.

Trial mold cost and acceptance terms: How to stipulate in the foreign trade mold contract

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1484.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.