The core contradiction of manifold molds is the filling of long flow channels and deformation of thin walls, with gate position and mold temperature being key variables.
1、 The gate position determines the filling endpoint
The intake manifold mold often adopts single point or double point pouring, and it is recommended to use double points when the channel length exceeds 250 millimeters.
When pouring at a single point, the end pressure loss can reach 30%, and insufficient filling is prone to occur at the end.
The double point pouring spacing is set equally according to the airway, and the end filling integrity rate can be increased by about 15%.
2、 Wall thickness and filling speed
The wall thickness of the manifold is usually 3 to 5 millimeters, and a filling time of 0.12 to 0.20 seconds is more reliable.
When the filling speed is below 1.5 meters per second, the probability of cold insulation increases by about 25%.
If the speed is higher than 3.5 meters per second, there will be air entrainment, which needs to be optimized in conjunction with exhaust synchronization.
3、 Mold temperature and deformation control
The temperature of the manifold mold is set at 280 to 320 degrees Celsius, with a temperature difference controlled within plus or minus 10 degrees Celsius.
Uneven mold temperature can cause the flange surface of the manifold to warp by more than 1.2 millimeters, resulting in air leakage during assembly.
Xinfeng arranges cooling on the manifold mold according to the air duct partition, and the flange surface can be compressed to within 0.8 millimeters.
4、 Exhaust and Internal Quality
The exhaust groove is located at the end of the flow channel and at the corner of the airway, with a groove depth of 0.2 to 0.25 millimeters.
The exhaust area shall be configured according to the projection of the cavity, with a minimum of 7 square millimeters per 100 square centimeters.
When the exhaust is insufficient, the internal porosity will increase to over 3%, which affects the airtightness.
5、 Verification and foreign trade demand
The manifold components need to undergo air tightness testing, with a pressure range of 0.1 to 0.15 megapascals and a holding time of 30 seconds.
European customers often require a cleanliness report for the internal cavity, with residue content limits typically below 50 milligrams per piece.
The demand for manifolds in new energy hybrid vehicles continues, and inquiries for matching molds are growing rapidly in the Southeast Asian market.
Conclusion and Outlook
The filling and deformation of manifold molds are two sides of the same thermal equilibrium problem.
First, determine the number of gates, then calibrate the mold temperature zone, and finally conduct airtightness verification. The number of repairs is usually reduced by one round.
Extension: Three parts of the manifold mold are prone to losing control
Insufficient exhaust at the airway angle can increase the end porosity to over 3%.
The flange surface cooling is too strong, resulting in an increase in warpage. It is necessary to adjust the temperature synchronously with the rod.
The residual root of the gate is too large, which increases the polishing time by about 15% and affects the cleanliness of the inner cavity.
The temperature zone of the mold is less than three zones, and the temperature difference at the transition between thin and thick layers often exceeds 12 degrees Celsius.
The air tightness test was not conducted during the trial mold, and the leakage was only discovered after mass production, doubling the rework cost.
Three areas are controlled in advance, and the first pass rate of manifold components is usually increased by about 15 percentage points.
Addendum: Three structural suggestions for manifold molds
It is recommended to use a quick change structure for airway inserts, with a single replacement time controlled within 1 hour.
The machining allowance of the flange surface is often taken as 2 millimeters, and if it is too thin, local black skin will appear after machining.
When the first piece of airtightness is not qualified, first check the density near the gate, and then check the residue inside the cavity.
FAQ
Should the manifold be poured at a single point or a double point? It is recommended to use double points for channels longer than 250 millimeters.
What is the filling time? Usually 0.12 to 0.20 seconds.
What happens if the charging speed is too low? The probability of a cold insulation of less than 1.5 meters per second increases.
How much is the flange surface warping controlled? Suggest within 0.8 to 1.2 millimeters.
How deep is the exhaust groove? 0.2 to 0.25 millimeters.
What is the pressure for airtight testing? Maintain a pressure of 0.1 to 0.15 megapascals for 30 seconds.
What is the limit for the cleanliness of the internal cavity? The residue is usually less than 50 milligrams per piece.
Subframe mold: casting system and tooling coordination for large aluminum castings
Moldes para fundição por baixa pressão (LPDC)
Moldes para fundição por gravidade
Moldes para fundição por contrapressão (CPC)
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda
MOLDES PARA JANTES AUTOMÓVEIS
PEÇAS ESTRUTURAIS AUTOMÓVEIS
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO
PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO
Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.