Perguntas frequentes

The subframe mold is a large-scale fixture, and the combination of the pouring system and the press fixture determines the single piece cycle time and qualifica

  • Vistas: ...
  • Tempo de liberação: 2026-11-16

The subframe mold is a large-scale fixture, and the combination of the pouring system and the press fixture determines the single piece cycle time and qualification rate.

1、 The pouring system is allocated according to the process

The sub frame casting weighs 8 to 12 kilograms, and the pouring system is often poured at 2 to 4 o'clock to ensure a balanced process.

When the process difference exceeds 15%, cold insulation and undercasting are prone to occur at the remote end.

The ratio of sprue to sprue area is often taken as 1:1.8 to 1:2.2 to avoid excessive pressure loss.

2、 Die stiffness and clamping

The wall thickness of the large mold cavity is about 15% thicker than that of the general mold, which suppresses filling deformation.

Insufficient clamping force can cause the flash thickness to exceed 0.5 millimeters, increasing the polishing time by about 20%.

The weight of the mold often reaches 3 to 6 tons and needs to be matched with the size of the press table and the pushing force.

3、 Cooling and rhythm

The sub frame mold is often equipped with point cooling at key nodes, which can shorten the cooling time of a single piece by about 12%.

The temperature difference on the mold surface should be controlled within plus or minus 8 degrees Celsius. Exceeding this limit will result in a hardness difference of more than 18HB for the same component.

Xinfeng uses embedded cooling inserts on the subframe mold, resulting in a local hot spot temperature drop of approximately 25 degrees Celsius.

4、 Deformation and shape correction

After demolding the subframe, there is often a deformation of 0.5 to 1.5 millimeters, and a calibration station needs to be reserved.

After heat treatment, the size will drift by about 0.3%, and the mold cavity should be pre compensated.

When the calibration process is missing, the deviation rate of the loading fit clearance increases by about 20%.

5、 Verification and Market

The first piece requires three-dimensional full-size with X-ray, and the flatness of the key connection surface should be controlled within 0.2 millimeters.

Mexican and Eastern European customers have seen a rapid increase in inquiries for subframe molds, with a focus on supporting new energy vehicle models.

Overseas projects often require the mold and tooling to be handed over together, and the interface standards need to be confirmed in advance.

Conclusion and Outlook

The production capacity of large component molds is determined by cooling and tooling, and structural strength is usually not the bottleneck.

By prioritizing process allocation, cold layout, and shaping workstations, the climbing cycle can be shortened by about three weeks.

Extension: Three Experiences in Transportation and Installation of Large Molds

When the weight of the mold exceeds 3 tons, it is necessary to calculate the rated load of the lifting point and workshop crane.

The wooden box base is designed to bear 1.2 times the weight of the mold to avoid deformation during transportation.

Apply anti rust oil to the mold cavity before transportation and tighten it to prevent long-distance vibration displacement.

During installation, check the parallelism of the press table. A deviation of more than 0.1 millimeters can cause uneven loading.

The initial heating should increase by 50 degrees Celsius per hour to avoid thermal shock cracking.

After implementing the three experiences, the installation and debugging time can usually be compressed by 2 to 3 days.

Addendum: Three key points for using subframe molds

It is recommended to install a filter screen on the pouring cup to reduce impurities by about 30%.

Before closing the mold, it is necessary to verify the pushing force. Insufficient pushing force will cause deformation and expansion of approximately 0.5 millimeters during demolding.

Before long-distance transportation, a compression plate is installed in the mold cavity, and displacement will cause the gap between the molds to widen, which was only discovered during mold testing.

FAQ

At what time does the subframe need to be poured? Usually from 2 to 4 o'clock, the process deviation is controlled within 15%.

What is the ratio of pouring area? Commonly used ratios range from 1:1.8 to 1:2.2.

How thick does the edge need to be polished? When it exceeds 0.5 millimeters, additional processing is required.

How much beat can a little cold shorten? Single piece cooling is reduced by about 12%.

How much is the temperature difference controlled on the mold surface? Within plus or minus 8 degrees Celsius.

Do you want to reserve a shaping workstation? Yes, the demolding deformation often reaches 0.5 to 1.5 millimeters.

What should I pay attention to when handing over keys overseas? Confirm the compressor interface and tooling standards in advance.

Export of Aluminum Alloy Wheel Casting Molds: Which Markets Have More Abundant Demand

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1477.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.