1、 Charging speed and entrainment

The filling time of thin-walled parts should be controlled between 0.15 and 0.25 seconds. If it is too slow, it will cause cold insulation, and if it is too fast, it will cause air entrapment.

When the speed of the sprue exceeds 3 meters per second, the defect rate of rolled air increases by about 18%.

The control arm mold often uses multi-point pouring, with a spacing of 60 to 80 millimeters between pouring points for a more balanced approach.

2、 Top out and deformation

The arrangement of the ejector pin should avoid the force bearing rod, and the synchronization error of the ejector should be controlled within 0.1 millimeters.

Uneven top out force can cause thin-walled components to warp by more than 1.5 millimeters, resulting in gaps during assembly.

Xinfeng sets up ejector pins on the control arm mold according to the rod section area, and the deflection can be compressed to within 1 millimeter.

3、 Dimensional compensation after heat treatment

After T6 heat treatment, the control arm will shrink by about 0.2% to 0.4%, and the mold cavity needs to be pre filled with compensation.

The hole spacing deviation of uncompensated molds after heat treatment may reach 0.5 millimeters or more.

The compensation amount is calibrated based on the measured material and wall thickness, usually determined through two rounds of mold testing.

4、 Mold temperature and exhaust

The mold temperature in the thin-walled area is set at 300 to 330 degrees Celsius, and the mold temperature fluctuation is controlled within plus or minus 8 degrees Celsius.

The total cross-sectional area of the exhaust groove shall not be less than 10 square millimeters per 100 square centimeters based on the projected area of the cavity.

When the exhaust is not smooth, the probability of insufficient filling at the end of the control arm increases by about 25%.

5、 Validation and Batch Production

The first piece can only be released if it meets the standards of three coordinate and X-ray, warpage and porosity.

During the batch stage, one piece will be sampled every 300 pieces, and the sampling will be relaxed after three consecutive batches pass.

Industry practice has shown that synchronous optimization of mold temperature and ejector can increase the yield of control arms by about 12 percentage points.

Conclusion and Outlook

The qualification rate of thin-walled parts is jointly determined by filling, ejection, and compensation, and any missing item will result in rework.

Writing the heat treatment shrinkage amount into the mold design input can save one round of mold testing.

Extension: Three common types of deviations in thin-walled test molds

The warpage exceeds 1.5 millimeters, often due to uneven top out force rather than incorrect cavity size.

Undercasting at the end is often misdiagnosed as a small gate, but in reality, it is mostly due to insufficient exhaust.

The deviation of the hole spacing after heat treatment exceeds 0.5 millimeters, indicating that the shrinkage compensation has not been calibrated according to actual measurements.

When the temperature fluctuation exceeds 10 degrees Celsius, the size drift of the same batch of parts is significant.

The lack of temperature curve in the trial mold record makes it difficult to reproduce the problem, and the rectification cycle is often extended by one week.

Three types of deviations are checked in order, and rectification can usually be compressed to 3 to 5 days.

Addendum: Three structural details of the control arm mold

The diameter of the top pin is usually taken as 8 to 12 millimeters. If it is too thin, it is easy to penetrate the thin-walled area, while if it is too thick, it will leave obvious marks.

It is recommended to add local reinforcement bars to the bent part of the rod, and the bending amount can be further reduced by about 0.3 millimeters.

If the end of the first piece is undercast, the exhaust should be checked first and then the gate should be checked. Reversing the order usually consumes an extra round of mold testing.

FAQ

How long does it take to control the arm filling time? Usually 0.15 to 0.25 seconds.

What is the upper limit of the sprue speed? There is a significant increase in air entrainment beyond 3 meters per second.

How much is the warpage controlled to? Suggest within 1 millimeter, exceeding 1.5 millimeters will affect assembly.

How much does heat treatment shrink? About 0.2% to 0.4% after T6.

Do we need to add compensation to the cavity? Required, calibrated according to material and wall thickness measurements.

How much is the mold temperature? Thin walled area at 300 to 330 degrees Celsius.

How is the exhaust area calculated? The projected area per 100 square centimeters shall not be less than 10 square millimeters.

Transmission case mold: exhaust and cleaning design for complex cavities

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1473.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.