Perguntas frequentes

CPC reverse pressure casting mold: How to achieve porosity below 0.8%

  • Vistas: ...
  • Tempo de liberação: 2026-11-16

CPC reverse pressure casting mold: How to achieve porosity below 0.8%

CPC reverse pressure casting reduces the porosity of castings to below 0.8%, relying on three factors: sealing, pressure curve, and exhaust accuracy.

1、 Sealing the cavity is a prerequisite

The flatness of the sealing surface of the cavity of the CPC reverse pressure casting mold needs to be controlled within 0.02 millimeters, otherwise pressure leakage may occur.

When the seal fails, insufficient backpressure is established, and the porosity of the casting will rise to over 2%.

The sealing ring is made of materials that can withstand temperatures above 300 degrees Celsius, and a single mold is usually equipped with two redundant seals.

2、 The pressure curve determines the filling quality

The back pressure is often set at 0.8 to 1.2 megapascals, and when it is lower than 0.6 megapascals, the shrinkage effect is significantly weakened.

The pressure gradient during the filling stage is controlled at 0.05 megapascals per second, and if it is too fast, it will generate gas entrainment.

The holding time is set at 3 to 4 seconds per millimeter of casting wall thickness. If it is too short, it will leave concentrated shrinkage holes.

3、 The accuracy of the exhaust groove affects the internal quality

The depth of the CPC mold exhaust groove is taken as 0.10 to 0.15 millimeters, which is shallower and more accurate than conventional low-pressure molds.

The total length of the exhaust groove shall be configured to be no less than 120 square millimeters per meter of the cavity circumference, and the position shall correspond to the final filling area.

Xinfeng simulated the final filling position on the CPC mold using CAE, and positioned the exhaust groove once, reducing the trial mold repair rate by about 20%.

4、 Mold temperature and aluminum liquid cleanliness

The temperature difference of the mold surface is controlled at plus or minus 5 degrees Celsius, and when the temperature difference expands to 15 degrees Celsius, the porosity increases by about 0.5 percentage points.

The hydrogen content of aluminum liquid after degassing should be controlled below 0.10 milliliters per 100 grams, which is the basis for high-grade flaw detection.

The pouring temperature is usually between 700 and 720 degrees Celsius. If it is too high, suction will occur, and if it is too low, insufficient filling will occur.

5、 Acceptance and Cost

The second level flaw detection requires that the area of a single defect should not exceed 3 square millimeters and should not be concentrated in the stress zone.

CPC mold investment is about 1.5 to 1.8 times higher than LPDC of the same specification, suitable for projects with an annual output of over 100000 pieces.

Industry practice has shown that the waste rate of CPC technology can be controlled within 1.2%, which has cost advantages after long-term amortization.

Conclusion and Outlook

Porosity is the result, sealing, curve, and exhaust are processes, and any failure to meet these standards cannot be achieved.

For high-end wheel hub and steering knuckle projects, it is recommended to conduct CAE and sample verification before mass production.

Extension: Three practical limitations in CPC promotion

The equipment investment is relatively high, and a single set of backpressure system often costs hundreds of thousands of yuan, which is difficult for small-scale factories to digest.

Seals are consumables, and the annual replacement cost can reach about 5% of the mold cost.

The tolerance of the exhaust groove needs to be controlled within plus or minus 0.01 millimeters, which is difficult for ordinary processing equipment to achieve stably.

When the cleanliness of the aluminum liquid does not meet the standard, the porosity advantage of CPC will be offset by about half.

The pace is slow, and the single piece time is often 20 to 30 seconds longer than LPDC. Capacity planning needs to be adjusted synchronously.

For projects with an annual output of less than 100000 pieces, it is recommended to first conduct cost estimation before deciding whether to adopt CPC technology.

FAQ

How much porosity can CPC achieve? The standardized process can be as low as 0.8% or less.

What is the appropriate counter pressure? Usually take 0.8 to 1.2 megapascals.

How deep is the exhaust groove? 0.10 to 0.15 millimeters, shallower than low-pressure molds.

How much is the temperature difference controlled on the mold surface? Within plus or minus 5 degrees Celsius.

What is the hydrogen content requirement for aluminum liquid? Less than 0.10 milliliters per 100 grams.

Sítio Web Deste artigo: https://pt.zj-xinfeng.com/case/1470.html

Get a Custom Product Proposal Online

Please fill out the form below to receive this for free.

Global Hotline:

+86-15356852630,13967513266

Moldes para fundição por baixa pressão (LPDC) 
Moldes para fundição por gravidade 
Moldes para fundição por contrapressão (CPC) 
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda

MOLDES PARA JANTES AUTOMÓVEIS 
PEÇAS ESTRUTURAIS AUTOMÓVEIS 
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO

NOTÍCIAS DA EMPRESA
NOTÍCIAS DO SETOR
BLOG TÉCNICO
PERGUNTAS FREQUENTES

PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO

Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.