Perform four checks during the assembly phase: mold clearance, ejection synchronization, water pressure measurement, and action interlocking.
1、 Closing gap
After the mold is closed, the gap between the parting surfaces should be less than 0.05 millimeters, and a feeler gauge should be used to check each section.
A gap exceeding 0.1 millimeters can cause excessive flash thickness and increase polishing time by about 20%.
The offset load of the mold needs to be eliminated by adjusting the guide column and cushion block, and force cannot be applied.
2、 Top out synchronization
The synchronization error of multi pin ejection is controlled within 0.1 millimeters to avoid deformation of thin-walled parts.
The ejection stroke and reset signal need to be interlocked to prevent mold collision.
The clearance between the top pin and the cavity is set at 0.03 to 0.05 millimeters, and it also serves as an auxiliary exhaust.
3、 Waterway pressure measurement
After assembly, the waterway needs to undergo a 0.6 megapascal pressure test, with a pressure drop of no more than 5% within 30 minutes.
The leakage at the joint and seal should be replaced immediately to avoid interruption of water leakage during mold testing.
The flow rate needs to be measured one by one, with a deviation controlled within 10%.
4、 Action and safety interlock
Core pulling, mold opening and closing, ejection, and spraying are interlocked in sequence to prevent interference.
The safety grating and emergency stop circuit need to be verified before the trial mold.
Electrical components must comply with the regulatory requirements of the customer's location.
5、 Confirmation before the first trial
Confirm that the mold lifting point, insulation sleeve interface, and press parameters are consistent.
Xinfeng completes the assembly inspection checklist before leaving the factory and provides inspection records along with the goods.
Industry data shows that for molds with complete assembly inspection, the success rate of the first trial mold is about 30% higher.
Conclusion and Outlook
The majority of trial mold failures are not due to process issues, but rather assembly details.
The four aspects of clearance, synchronization, pressure testing, and interlocking have been passed, and the success rate of the first test has been significantly improved.
Extension: Three preparations on the day of trial molding
Preparation 1: The temperature of the aluminum liquid should be stabilized within the target window of plus or minus 5 degrees Celsius in advance.
Preparation II: mold preheating is increased by 50 ℃ per hour to avoid thermal shock.
Preparation 3: Testing tools and flaw detection equipment are in place, and the first piece is immediately inspected.
One of the three preparations is missing, and on the day of the trial, it often takes half a day to complete.
The first article inspection results are recorded on the spot, making problem localization faster.
Xinfeng provides a trial mold preparation checklist before delivery for the customer's production line to verify.
Addendum: Five verifications for assembly and debugging
Before closing the mold, a short loop test is required to significantly reduce the probability of incorrect action sequence.
Insufficient lubrication of the guide column will increase the clamping resistance and widen the gap accordingly.
The reset signal must be confirmed before closing the mold, otherwise there is a risk of mold collision.
It is recommended to conduct water pressure testing under insulation conditions, as joint leakage is more likely to be exposed.
Take photos and record the initial state before the first test, which is convenient for comparison and judgment in case of abnormalities.
Addendum 2: Two benchmarks for assembly accuracy
The clearance between the guide post and the guide sleeve should be set at 0.02 to 0.04 millimeters, as excessive clearance can affect the precision of the mold.
The mating surface needs to be inspected with red lead, and if the contact surface is below 80%, further grinding is required.
Addendum 3: Two records of mold closing and debugging
The gap distribution should be recorded for the first mold closing to facilitate comparison with subsequent wear.
The number of ejection times and reset time need to be recorded, and any abnormalities can be detected in advance to determine the status of the mechanism.
FAQ
How much is the gap control on the parting surface? Less than 0.05 millimeters.
What are the effects of a large gap? Thick flying edge increases polishing time by about 20%.
What is the synchronization error of the top out? Control within 0.1 millimeters.
What is the clearance between the top pins? 0.03 to 0.05 millimeters.
Water pressure measurement parameters? Maintain a pressure of 0.6 megapascals for 30 minutes, with a pressure drop not exceeding 5%.
Do we need to do action interlocking? It is necessary to prevent collision interference.
How much can the success rate of the first attempt be improved? About 30%.
Small batch and multiple varieties: How to dilute mold investment
Moldes para fundição por baixa pressão (LPDC)
Moldes para fundição por gravidade
Moldes para fundição por contrapressão (CPC)
Moldes para fundição de peças estruturais
Molde para fundição de cubos de roda de motocicleta
Molde para fundição por pressão diferencial de cubos de roda
Molde para fundição por gravidade de cubos de roda
Molde para fundição por baixa pressão de cubos de roda
MOLDES PARA JANTES AUTOMÓVEIS
PEÇAS ESTRUTURAIS AUTOMÓVEIS
OUTROS COMPONENTES DE FUNDIDOS DE ALUMÍNIO
PERFIL DA EMPRESA
ESTRUTURA ORGANIZACIONAL
HISTÓRICO DE DESENVOLVIMENTO
PROPRIEDADE INTELECTUAL
ESPÍRITO DE EQUIPA PARCEIRO
Copyright © Zhejiang Xinfeng Machinery Co., Ltd. All Rights Reserved.